房子裝修后有些會(huì)出現(xiàn)起皮、掉粉、開裂等問(wèn)題,尤其是頂棚樓板接縫處更為明顯。今天我們就來(lái)盤點(diǎn)一下膩?zhàn)臃鄢R?jiàn)的表面脫粉問(wèn)題以及解決方法。
After the house is decorated, some problems such as peeling, powder falling and cracking will appear, especially at the joints of the ceiling and floor slab. Today, let's take stock of the common surface de dusting problems of putty powder and their solutions.
產(chǎn)生原因:
Cause:
1、施工原因:由于油漆師傅在后一道收光施工時(shí)多次用刮刀干刮墻面而引起的表面細(xì)微的起皮現(xiàn)象,等干燥后就會(huì)形成脫粉癥狀。
1. Construction reason: the subtle peeling phenomenon on the surface caused by the painter repeatedly scraping the wall with a scraper during the subsequent finishing construction will form a powder removal symptom after drying.
2、人為原因:由于后一道施工膩?zhàn)游锤蓵r(shí),遇到外來(lái)粉塵附著到墻面上(切割作業(yè),大風(fēng),清理地板等)導(dǎo)致的墻面假象脫粉。
2. Human reason: the false appearance of wall surface de dusting caused by foreign dust adhering to the wall surface (cutting operation, strong wind, floor cleaning, etc.) when the later construction putty is not dry.
3、生產(chǎn)原因:由于生產(chǎn)人員粗心將原料配方比例放錯(cuò),或因機(jī)臺(tái)設(shè)備故障,導(dǎo)致的配方不穩(wěn)定而引起的脫粉。
3. Production reason: the production personnel carelessly put the wrong proportion of raw material formula, or the formula is unstable due to machine equipment failure, which leads to the de powdering.
![濟(jì)南膩?zhàn)臃? src=]()
處理方法:
Treatment method:
1、施工師傅在做后一道不上漆收光施工時(shí)應(yīng)注意膩?zhàn)拥谋砻鏉穸?,太干時(shí)會(huì)引起起皮脫粉,在收光時(shí)將刀痕修平即可,不宜多次干刮。
1. The construction master should pay attention to the surface humidity of the putty when finishing without painting. If it is too dry, it will cause peeling and powdering. When finishing, just flatten the knife marks, and it is not suitable to dry scrape for many times.
2、如出現(xiàn)粉塵附著在墻面上造成的假象脫粉的,應(yīng)待裝修完畢后用雞毛撣清除粉塵,或用清水與干凈的布條擦拭干凈即可。
2. If there is a false appearance of dusting caused by dust adhering to the wall, you should remove the dust with a feather duster after the decoration, or wipe it with clean water and clean cloth.
3. In case of quick drying and de powdering of Jinan putty powder, it is necessary to wait for the company's technicians to come to the site to identify whether it is caused by the product formula.
如果是產(chǎn)品配方問(wèn)題出現(xiàn)的癥狀應(yīng)是:批刮時(shí)不好批刮,快干,干透以后膩?zhàn)訉颖容^松,易脫粉,易龜裂等現(xiàn)象。更多相關(guān)事項(xiàng)就來(lái)我們網(wǎng)站
http://www.chnzylw.com咨詢吧。
If it is a product formula problem, the symptoms should be: it is not easy to scrape when scraping, fast drying, and the putty layer is relatively loose after drying, easy to remove powder, easy to crack and so on. Come to our website for more related matters http://www.chnzylw.com Consult.