濟南膩子粉有色差和脫粉的原因與處理辦法

來源:http://www.chnzylw.com 日期:2024-12-07 發(fā)布人:

  有色差

  There is a color difference

  產(chǎn)生原因石膏粉

  Cause of occurrence

  1、膩子粉本身屬于半成品,原材料不穩(wěn)定是導(dǎo)致色差的主要原因之一,由于礦區(qū)開采出來的礦粉會因區(qū)域不同而品質(zhì)不同,如未注意調(diào)配,就會出現(xiàn)各個批次不同而色差。

  1. Putty powder itself is a semi-finished product, and the instability of raw materials is one of the main reasons for color difference. Due to the different quality of mineral powder extracted from mining areas, if not properly mixed, color difference may occur in different batches.

  2、由于有些廠家使用“濫竽充數(shù)”的方法將低等級原料混雜發(fā)貨,因為采購的數(shù)量較大,無法逐一抽檢到位,導(dǎo)致有個別“漏網(wǎng)之魚”參雜在生產(chǎn)里面導(dǎo)致個別性的色差。

  2. Due to some manufacturers using the method of "filling numbers with inferior materials" to mix and ship low-grade materials, the large quantity purchased cannot be inspected one by one, resulting in individual "missed fish" mixed in production and causing individual color differences.

  3、由于生產(chǎn)人員失誤將不同等級的原料參雜在一起生產(chǎn)引起的色差或?qū)⒉煌放频漠a(chǎn)品批刮在同一面墻上而引起的色差。

  3. Color difference caused by production personnel mistakenly mixing different grades of raw materials together or scraping different brands of products on the same wall.

  處理方法

  processing method

  1、色差一般不是配方問題,所以不存在質(zhì)量問題,如要上漆的墻面一般是可以用漆膜遮蓋過去,不會影響整體裝飾效果,如一般批刮二、三道不上漆的墻面出現(xiàn)色差,建議其再批刮一道無色差的膩子粉或上漆。

  1. Color difference is generally not a formula issue, so there is no quality problem. For walls that need to be painted, they can generally be covered with paint film without affecting the overall decorative effect. If color difference occurs when scraping two or three layers of unpainted walls, it is recommended to scrape another layer of colorless putty or paint.

  2、所有參與生產(chǎn)及施工的人員應(yīng)嚴格按照有關(guān)標準進行生產(chǎn)和施工,避免產(chǎn)生人為的質(zhì)量問題。

  2. All personnel involved in production and construction should strictly follow relevant standards to avoid human caused quality problems.

  脫粉

  De powdering

  產(chǎn)生原因

  Cause of occurrence

  1.施工原因:由于油漆師傅在最后一道收光施工時多次用刮刀干刮墻面而引起的表面細微的起皮現(xiàn)象,等干燥后就會形成脫粉癥狀。

  1. Construction reason: Due to the painter's repeated use of a scraper to dry scrape the wall surface during the final finishing process, there is a slight peeling phenomenon on the surface, which will cause powdering symptoms after drying.

  2.人為原因:由于最后一道施工膩子未干時,遇到外來粉塵附著到墻面上(切割作業(yè),大風(fēng),清理地板等)導(dǎo)致的墻面假象脫粉。

  2. Human factors: Due to the last layer of construction putty not drying yet, external dust adhered to the wall surface (cutting operations, strong winds, cleaning floors, etc.), causing the wall surface to appear powdery.

  3.生產(chǎn)原因:由于生產(chǎn)人員粗心將原料配方比例放錯,或因機臺設(shè)備卸漏,導(dǎo)致的配方不穩(wěn)定而引起的脫粉。

  3. Production reasons: Powder shedding caused by unstable formula due to careless placement of raw material formula ratios by production personnel or leakage of machine equipment.

  處理方法

  processing method

  1.施工師傅在做最后一道不上漆收光施工時應(yīng)注意膩子的表面濕度,太干時會引起起皮脫粉,在收光時將刀痕修平即可,不宜多次干刮。

  1. The construction master should pay attention to the surface humidity of the putty when doing the last unpainted finishing construction. If it is too dry, it will cause peeling and powdering. When finishing, the knife mark can be smoothed out, and it is not advisable to dry scrape it multiple times.

  2.如出現(xiàn)粉塵附著在墻面上造成的假象脫粉的應(yīng)待裝修完畢后用雞毛彈清除粉塵,或用清水與干凈的布條擦拭干凈即可。

  If dust adheres to the wall and causes false detachment, it should be removed with a chicken feather ball after decoration is completed, or wiped clean with water and a clean cloth strip.

  3.如出現(xiàn)快干脫粉的,應(yīng)等公司技術(shù)人員到現(xiàn)場鑒定是否是由于產(chǎn)品配方引起的原因。

  3. If there is fast drying and powdering, the company's technical personnel should wait on site to identify whether it is caused by the product formula.

  本文由 濟南膩子粉 友情奉獻.更多有關(guān)的知識請點擊  http://www.chnzylw.com   真誠的態(tài)度.為您提供為全面的服務(wù).更多有關(guān)的知識我們將會陸續(xù)向大家奉獻.敬請期待.

  This article is a friendly contribution from Jinan Putty Powder For more related knowledge, please click http://www.chnzylw.com Sincere attitude To provide you with comprehensive services We will gradually contribute more relevant knowledge to everyone Coming soon.

???